MARGINAL FIDELITY AND FRACTURE STRENGTH OF IPS EMPRESS $2^{(R)}$ CERAMIC CROWNS ACCORDING TO DIFFERENT CEMENT TYPES

Cho Hyun-Ok    (Dept. of Prosthodontics, College of Dentistry, Chosun University   ); Kang Dong-Wan    (Dept. of Prosthodontics, College of Dentistry, Chosun University  );
  • 초록

    There has been increasing use of IPS Empress $2^{(R)}$ owing to easy fabrication method, high esthetics similar to natural teeth, good marginal accuracy, and sufficient fracture strength. However, in clinical application, although a luting agent and the tooth cementation bonding procedure influence the marginal accuracy and fracture strength restoration, there has been a controversy in the selection of proper luting agent. This study was to measure the marginal fidelites and fracture strength of IPS Empress crowns according to three cement types, Protec $cem^{(R)}$ , Variolink $II^{(R)}$ and Panavia $21^{(R)}$ . After construction of 12 experimental dies for each group, IPS Empress $2^{(R)}$ crowns were fabricated and luted the metal master die prepartion of the maxillary right premolar. Marginal gaps before cementation and after cementation were measured. Buccal incline on the functional cusp of specimens were loaded until the catastrophic failure and fracture strength was measured. The results of this study were as follows: 1. The range of gap was $34.04{\pm}4.84{\mu}m$ before cementation and $37.88{\pm}5.00{\mu}m$ after cementation, which showed significant difference by paired t-test (p 0.05). 2. The difference in the results from marginal accuracy according to three cement types Proved that The Variolink $II^{(R)}$ cement group had the least gap, $35.43{\pm}5.03{\mu}m$ , and showed superior marginal accuracy while there existed statistic significance in Protec $cem^{(R)}$ cement group, $39.06{\pm}4.41{\mu}m$ or Panavia $21^{(R)}$ cement group, $39.16{\pm}4.39{\mu}m$ by two-way ANOVA test & multiple range test (p $II^{(R)}$ cement group shows highest fracture strength of $1257.33{\pm}226.77N$ , Panavia $21^{(R)}$ cement group has $1098.08{\pm}138.45N$ , and Protec $cem^{(R)}$ cement group represents the lowest fracture strength of $926.75{\pm}115.75N$ . 4. Three different cement groups of different components showed acceptable marginal fidelity and fracture strength. It is concluded that IPS Empress $2^{(R)}$ crowns luted using Variolink $II^{(R)}$ cement group had stronger fracture strength and smaller marginal gap than the other cement groups. Although Variolink $II^{(R)}$ resin cement seemed acceptable to clinical applications in IPS Empress $2^{(R)}$ system, the IPS Empress $2^{(R)}$ system still requires long-term research due to the lack of data in clinical applications.


  • 주제어

    All ceramics .   luting agent .   marginal accuracy .   fracture strength.  

  • 참고문헌 (30)

    1. Ferrai, M.. 'Cement Thickness and Microleakage leakage under Dicor Crowns.' Int J. Prosthet, 4:126-131, 1991 
    2. Malament, K.A. Grossman, D.G.. 'Clinical application of bonded Dicor crown(IADR abstract 1523).' J Dent Res., 69(special issue):299, 1990 
    3. Rosenstiel, S.F. Land, M.F. Crispin, B.J.. 'Dental Luting Agents: A review of the current literature.' J Prosthet Dent,. 80:280, 1998 
    4. Holmes, J.R Sulik, W.D. Hall, G.A. Bayne, S.C.. 'Marginal fit of castable ceramic crowns.' J Prosthet Dent., 67:594-599, 1992 
    5. Leevailoj, C. Platt, J.A. Cochran, M.A. Moore, B.K.. 'In vitro study of fracture incidence and compressive fracture load of all-ceramic crowns cemented with resin modified glass ionomer and other luting agents.' J Prosthet Dent., 80:699-707, 1998 
    6. Jensen, J.E. Sheth, J.J. Tolliver, D.. 'Etched-porcelain resin-bonded full-veneer crowns. In vrtro fracture resistance.' Compend Cantin Educ Dent., 10:336-347, 1989 
    7. Burke, F.J.T..'The Effect of Variations in Bonding Procedure on Fracture Resistance of Dentine-Bonded All-Ceramic Crowns.' Quintessence Int., 26:293-300, 1995 
    8. Nevia, G. Yaman, P. Dennison, J.B.. 'Resistance to Fracture of Three All-ceramic Systems.' J Esthet Dent., 10:60, 1998 
    9. Grey, N.J.A. Piddock, V. Wilson, M.A..'In vitro comparison of conventional crowns and a new all-ceramic system.' J Dent., 21:47-51, 1993 
    10. Proster, L.. 'Compressive Strength of Two Modern All-Ceramic Crowns.' Int J Prosthet., 4: 409-414. 1992 
    11. Schweiger, M. Holand, W.. ' IPS Empress 2 :A New Pressable High-Strength Glass-Ceramic for Esthetic All-Ceramic Restoration.' QDT., 143, 1999 
    12. Bernal, G. Jones, M.R. Brown, D.T.. 'The Effect of Finish Line Form and Luting Agent On the Breaking Strength of Dicor Crowns.' Int J Prosthet., 6:286-290, 1993 
    13. Mito, W.T. Mito, Sorensen, J.A.. 'Fabrication of Fixed Partial Dentures with Empress 2.' QDT. 164, 1997 
    14. Rinke, S. Huls, A.. 'Marginal Accuracy and Fracture Strength of Conventional and Copy-Milled All Ceramic crowns.' Int J Prosthet., 8:303-310, 1995 
    15. Yoshinari, M. Derand, T.. 'Fracture strength of All-Ceramic Crowns.' Int J Prosthet., 7:329, 1994 
    16. Schneider, D.M. Levi, M.S. Mari, D.F.. 'Porcelain shoulder Adaptation using direct refractoary dies.' J Prosthet Dent., 36:583, 1976 
    17. Campbell, S.D.. 'A comparative strength study of metal ceramic and all-ceramic esthetic materials: modulus of rupture.' J Prosthet Dent., 62:476, 1989 
    18. Grossman, D.G. Nelson, J.W.. 'The bonded Dicor crown[IADR abstract 800].' J Dent Res., 66(special issue):206, 1987. 
    19. Marquis, P.M.. 'The Infulence of cements on the ma-chanical performance of dental ceramics.' Bioceramics. 5:317-546, 1993 
    20. Sozio, R.B. Riley, E.J.. 'The Shinkage-free ceramic crowns.' J Prosthet Dent., 49:182, 1983 
    21. Sorensen J.A.. 'A standardized method for determination of crown margin fidelity.' J Prosthet Dent., 64:18, 1990 
    22. De Boever, J.A. McCall, W.D. Holden, S. Ash, M.M.. 'Functional occlusal force: An investigation by telemetry.' J Prostet Dent., 40:326-333, 1978 
    23. Groten, M. Proster, L.. 'The Infulence of different Cementation Modes on the Fracture Resistance of Feldspathic Ceramic Crowns.' Int J Prosthodont., 10:169-177, 1997 
    24. Ferrai, M.. 'Cement Thickness and Microleakage leakage under Dictor Crowns.' Int J Prosthet. 4:126-131, 1991 
    25. Adair, P.J. Grassman, D.G.. 'The castable cermaic crown.' Int J periodont Rest Dent., 4:32, 1984 
    26. Land, C.. 'Porcelain dental arts.' Dent Comos., 45(8):615-620, 1903 
    27. Nathanson, D.. 'Principles of porcelain use an an inlay/onlay material.' Chicago:Quintessence., 32-37, 1994 
    28. Mclnnes-Ledoux, P.M. Ledoux, W.R. Weinberg, R.. 'A bond strength study of luted castable ceramic restorations.' J Dent Res., 68:823-825, 1989 
    29. Pera, P. Gilodi, S. Bassi,F. Carossa, S.. 'In vitro marginal adaption of alumina porcelain ceramic crowns.' J Prosthet Dent., 72:585-90, 1994 
    30. Sadoun, M.. 'All Ceramic bridges with the slip casting technique.' Presented at the 7th international symposium on ceramics, Paris, September, 1988 

 활용도 분석

  • 상세보기

    amChart 영역
  • 원문보기

    amChart 영역

원문보기

무료다운로드
유료다운로드
  • 원문이 없습니다.

유료 다운로드의 경우 해당 사이트의 정책에 따라 신규 회원가입, 로그인, 유료 구매 등이 필요할 수 있습니다. 해당 사이트에서 발생하는 귀하의 모든 정보활동은 NDSL의 서비스 정책과 무관합니다.

원문복사신청을 하시면, 일부 해외 인쇄학술지의 경우 외국학술지지원센터(FRIC)에서
무료 원문복사 서비스를 제공합니다.

NDSL에서는 해당 원문을 복사서비스하고 있습니다. 위의 원문복사신청 또는 장바구니 담기를 통하여 원문복사서비스 이용이 가능합니다.

이 논문과 함께 출판된 논문 + 더보기