Eco-Friendly Flame Retardant Poly(butylene terephthalate) Copolymers with Thermal Stability and Hydrolytic Resistance

Park, Jong-Min    (KOLON Central Research Park   ); Lee, Jun-Young    (School of Chemical Engineering, Sungkyunkwan University   ); Park, Yun-Heum    (School of Chemical Engineering, Sungkyunkwan University  );
  • 초록

    Eco-friendly flame retardant poly(butylene terephthalate) copolymers (FR-PBTs) were synthesized with various amounts (5.5, 8, 10 and 15%) of the flame retardant, phosphorous comonomer unit, [(6-oxido-6H-dibenz oxaphosphorin-6-yl)methyl]-methyl butanedioate (DOP-MBDA). Thermal stability was determined by TGA and the resistance to hydrolysis was examined by comparing the inherent viscosities of the polymers before and after hydrolysis in a 10 wt% aqueous NaOH solution at $130^{\circ}C$ for 8 h. Unfortunately the thermal stability and hydrolytic resistance of the copolymer decreased gradually with increasing DOP-MBDA content up to 10%. However, when the DOP-MBDA content was increased from 10 to 15% (FR-PBT-15), the thermal stability and hydrolytic resistance improved dramatically to those of the PBT homopolymer. FTIR spectroscopy showed that the ratio of the trans to gauche moiety in the copolymer chain decreased with increasing DOP-MBDA content up to 10%, whereas the ratio increased when 15% DOP-MBDA was incorporated into the polymer. The higher trans to gauche ratio suggests that crystallization may take place more readily in FR-PBT-15. In addition, FR-PBT-15 showed the highest density and degree of crystallinity among the copolymers. The improved thermal stability and resistance to hydrolysis of FR-PBT-15 was attributed to the denser stereo-stable crystal structure of the polymer.


  • 주제어

    poly(butylene terephthalate) copolymer .   phosporous flame retardant .   thermal stability .   hydrolytic stability.  

  • 참고문헌 (30)

    1. Alcan Chemicals, Plastics Additives & Compounding, 2, 24 (2000). 
    2. J. T. Yeh, S. H. Hsieh, Y. C. Cheng, M. J. Yang, and K. N. Chen, Polym. Degrad. Stabil., 61, 399 (1998). 
    3. C. M. Tai and R. K. Y. Li, Mater. Des., 22, 15 (2001). 
    4. J. Edenbaum, Plastics additive and modifiers handbook, Van Nostrand Reinhold Co., New York, 1992. 
    5. M. Day, T. J. Suprunchuk, D. Cooney, and D. M. Wiles, J. Appl. Polym. Sci., 33, 2041 (1987). 
    6. D. W. Van Krevelen, J. Appl. Polym. Sci. Appl. Polym. Symp., 31, 269 (1977). 
    7. V. Freudenberger and F. Jakob, Makromol. Chem., 105, 203 (1982). 
    8. E. M. Pearce, Y. P. Khanna, and D. Raucher, Thermal Characterization of Polymeric Materials, Academic Press, New York, 1983. 
    9. S. J. Chang and F. C. Chang, Polymer, 39, 3233 (1998). 
    10. A. Granzow and J. F. Cannelongo, J. Appl. Polym. Sci., 20, 689 (1976). 
    11. T. Suebsaeng and C. A. Wilkie, J. Polym. Sci., Polym. Chem. Ed., 22, 945 (1984). 
    12. S. J. Chang, Y. C. Sheen, R. S. Chang, and F. C. Chang, Polym. Degrad. Stabil., 54, 365 (1996). 
    13. C. S. Wang, J. Y. Shieh, and Y. M. Sun, Eur. Polym. J., 35, 1465 (1999). 
    14. K. Faghihi, M. Hajibeygi, and M. Shabanian, Macromol. Res., 17, 739 (2009).     
    15. D. Derouet, F. Morvan, and J. C. Brosse, J. Appl. Polym. Sci., 62, 1855 (1996). 
    16. Modern Plastics Encyclopedia, B-67, McGraw Hill, New York, 1995. 
    17. S. V. Levchik, G. F. Levchik, A. I. Balabanovich, E. D. Weil, and M. Klatt, Angew. Makromol. Chem., 264, 48 (1999). 
    18. G. F. Levchik, Y. V. Grigoriev, A. I. Balabanovich, S. V. Levchik, and M. Klatt, Polym. Int., 49, 1095 (2000). 
    19. J. M. Park and Y. H. Park, Macromol. Res., 13, 128 (2005).     
    20. K. S. Annakutty and K. Kishore, Polymer, 29, 756 (1988). 
    21. S. Sawada, K. Kamiyama, S. Ohgushi, and K. Yabuki, J. Appl. Polym. Sci., 42, 1041 (1991). 
    22. A. Kaito, K. Nakayama, and Zubaidi, J. Appl. Polym. Sci., 45, 1203 (1992). 
    23. D. A. Skoog and J. J. Leary, Principles of Instrumental Analysis, 4th ed., Harcourt Brace College Publisher, Florida, 1992, Chap. 12. 
    24. J. E. Mark, A. Eisenberg, W. W. Graessley, L. Mandelkern, E. T. Samulski, J. L. Koenig, and G. D. Wignall, Physical Properties of Polymers, 2nd ed., ACS, Washington D.C., 1993, Chap. 6. 
    25. J. S. Jang, J. H. Oh, and S. L. Moon, Macromolecules, 33, 1864 (2000). 
    26. D. L. Pavia, G. M. Lampman, and G. S. Kriz, Introduction to Spectroscopy, 2nd ed., Harcourt Brace College Publisher, Florida, 1996, Chap. 2. 
    27. S. Maki, E. Seiji, A. Yoshio, M. Go, G. Shoichi, and T. Hideo, J. Appl. Polym. Sci., 78, 1134 (2000). 
    28. C. Nguyen and J. H. Kim, Macromol. Res., 16, 620 (2008).     
    29. D. D. Schryver, S. D. Landry, and J. S. Reed, Polym. Degrad. Stabil., 64, 471 (1999). 
    30. G. Camino, G. Martinasso, and L. Costa, Polym. Degrad. Stabil., 27, 285 (1990). 

 활용도 분석

  • 상세보기

    amChart 영역
  • 원문보기

    amChart 영역

원문보기

무료다운로드
  • 원문이 없습니다.
유료다운로드

유료 다운로드의 경우 해당 사이트의 정책에 따라 신규 회원가입, 로그인, 유료 구매 등이 필요할 수 있습니다. 해당 사이트에서 발생하는 귀하의 모든 정보활동은 NDSL의 서비스 정책과 무관합니다.

원문복사신청을 하시면, 일부 해외 인쇄학술지의 경우 외국학술지지원센터(FRIC)에서
무료 원문복사 서비스를 제공합니다.

NDSL에서는 해당 원문을 복사서비스하고 있습니다. 위의 원문복사신청 또는 장바구니 담기를 통하여 원문복사서비스 이용이 가능합니다.

이 논문과 함께 출판된 논문 + 더보기